Gutpela-Tuning bilong yuMFDC Spot Welda: Wanpela Kwik Setap Gaid
Kisim ol gutpela weld wantaimnamel -frikwensi dairekt karent (MFDC) spot weldai nidim long skelim tripela ki seting:karent, taim, na presa. Em hia hau long ringim ol:

1. Stretim Nau: Kontrolim Hat
Stat long liklik: Long 0.8mm 'mild steel', stat long 200-300A.
Testim na skruim: Lepim karent long 10% step inap yu lukim:
✅ Ful nugget penetresen (no gat ol wik join)
❌ Nogat spata o paia-tru (i soim olsem i gat planti pawa)
Aluminium tip: Yusim 30-50% liklik karent winim ain bikos em i gat bikpela konduktiviti.
2. Taim bilong weldim: Bosim taim bilong hat
Ain: Sotpela taim + bikpela pawa (olsem, 3-6 seken @ 320A bilong M6 nat)
Aluminium/Kopa: Longpela taim + liklik pawa
Tok lukaut: Longpela taim tumas=elektrod i pas; Sotpela tumas=inkomplit fusen.
3. Presa bilong Elektrod: Mekim Gut Kontek
Ol liklik pepa (<1mm): 0.3-0.5 MPa
Thick plates (>3mm): 0.8-1.2 MPa
Kritikel resio: Inkrisim presa 5% long olgeta 10% 'current boost'.
Galvanized steel fix: Yusim bikpela o wankain olsem 0.6MPa presa long stopim 'zinc spatter'.
4. Mentenens bilong Elektrod: Konsistens em i bikpela samting
Ol toksave bilong sapim: Grindim olgeta 50-100 weld wantaim gutpela 'sandpaper'.
Mekim i kol gut: Sekim wara i ron long olgeta wik – ol 'soft electrode' i save kamapim 'drift'.
Anti-stick: Putim 'graphite paste' taim yu weldim aluminium.
Ol Pro Tip bilong Setim
- Test wanwan: Stretim wanpela paramita long wanpela taim.
- Stretim wankain pasin: Skelim 'nugget diameter' - 'variance'<0.2mm.
- Sevim ol profail: Putim ol gutpela seting bilong ol narapela narapela samting.
Trupela samting i kamap: Wanpela faktori i skruim laip bilong ol 'electrode' long 500 i go inap 1200 aua long rot bilong 'tip dressing' na 'cooling optimization' oltaim.
Kwik Refrens bilong stretim hevi
| Hevi | Ating stretim |
|---|---|
| Spatter | ↓ Karent o ↑ Presa |
| Slak Weld | ↑ Nau + ↑ Taim |
| Electrode Stick | ↓ Taim + Klin Tip |